Proposed Revisions To: Standard Specifications for Cast-in-Place nonreinforced concrete pipe (AC1 346-70)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposed Revisions To: Standard Specifications for Cast-in-Place nonreinforced concrete pipe (AC1 346-70)

Author(s): ACI Committee 346

Publication: Concrete International

Volume: 2

Issue: 8

Appears on pages(s): 65-70

Keywords: admixtures; aggregates; air entrainment; cast-in-place pipes; compressive strength; concrete construction; concrete pipes; curing; finishing; form-work (construction); joints (junctions);

DOI:

Date: 8/1/1980

Abstract:
These specifications cover construction of cast-in-place nonreinforced concrete pipe used for the conveyance of liquids such as irrigation water, storm water, sewage, and industrial wastes. These spec-ifications are a reference standard which the engineer or architect may make applicable to any cast-in-place pipe project by citing them in the project specifications.