Title: Conveying -A New Idea?

Author(s): James L. Cope

Publication: Concrete International

Volume: 2

Issue: 8

Appears on pages(s): 28-32

Keywords: concretes; concrete construction; convey-ing; placing; ready-mixed concrete.

DOI:

Date: 8/1/1980

Abstract:
This article reviews the development of three different ypes of conveyors for efficient placing of ready-mixed concrete. The first such conveyors were self-contained portable conveyors with limited lift, reach, and spreading capabilities. The next units developed were spreading conveyors; cantilevered conveyors for radial spreading and side discharge conveyors for straight line spreading. Finally series or feeder conveyors were developed which greatly ex-tended the reach and lift capacity of conveyors by using multiple units in combination or as a system for concrete placing. Recent developments are reported and predictions of future developments are made.