Use Less Cement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Use Less Cement

Author(s): Bryant Mather

Publication: Concrete International

Volume: 2

Issue: 10

Appears on pages(s): 22-24

Keywords: admixtures; air entrainment; cement con-tent; mass concrete; mix proportioning; water-cement ratio.

DOI:

Date: 10/1/1980

Abstract:
In a series of references and quotations, the author suggests that less cement can be used in certain cir-cumstances. Results of investigations suggest that mass concrete having appropriate levels of relevant properties for dam construction can be produced with cement quantities as low as 60 lb per cu yd (36 kglm3) and with water content of less than 80 lb per cu yd (48 kg/m3). Workable mixtures and compressive strengths are discussed as well as the need for investigating or modifying our present state of the art. It is suggested that special concrete mixtures should be priced ac-cordingly.