High-Strength Concrete: Past, Present, Future

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: High-Strength Concrete: Past, Present, Future

Author(s): Kenneth L. Saucier

Publication: Concrete International

Volume: 2

Issue: 6

Appears on pages(s): 46-50

Keywords: cement content; coarse aggregate; compressive strength; fly ash; high-strength concretes: plasticizers; research; reviews; slurries; water-cement ratio.

DOI:

Date: 6/1/1980

Abstract:
The paper summarized the current status of high-strength concrete, the research needed, and the information and experience required for high-strength concrete to become universally accepted. Discussion involves examination of three levels of high-strength concrete: (1) the present range of 5000 to 10,000 psi (34.4 to 68.9 MPa), (2) the available range of 10,000 to 15,000 psi (68.9 to 103.4 MPa), and (3) the exotic area of 15,000 psi (103.4 MPa). Present practices include use of low water-cement ratio, high cement factor, mixtures with fly ash, high quality crushed ag-gregates, high range water-reducing admixtures, and more coordination and quality control efforts. The second range is attainable with available materials and equipment such as slurry mixing, no-slump concrete, closer control, compaction by pressure, new admixtures, longer curing, and polymer material. Research in the areas of vibration and compaction, use of artificial aggregates, polymers, discontinuous reinforcement, interaction with the energy situation, and design considerations will be needed before the 15,000 psi (103.4 MPa) range can be successfully entered. The exotic area may include, heretofore, impractical techniques such as combining pressure and vibration and development of the silicalime bond. A prediction is offered of the technique to be used for the manufacture, placement, and consolidation of high-strength concrete in the year 2000.