Bemis Bag Plant in Winnipeg, Canada

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Bemis Bag Plant in Winnipeg, Canada

Author(s): Leonard K. Eaton

Publication: Concrete International

Volume: 1

Issue: 2

Appears on pages(s): 63-65

Keywords: beams (supports); columns (supports); concrete durability; concrete slabs; reinforced concrete,

DOI:

Date: 2/1/1979

Abstract:
The author describes the first large reinforced concrete structure in the Winnipeg area, built in the early 1900s. This factory building resulted in an important shift in construction technology in western Canada from conventional designs of the times to the more durable concrete material,