Concrete Houses Conserve Energy, Reduce Costs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Houses Conserve Energy, Reduce Costs

Author(s): Joseph A. Dobrowolski

Publication: Concrete International

Volume: 1

Issue: 9

Appears on pages(s): 27-31

Keywords: anchorage (structural); cement pastes; concrete construction; energy methods; fire resistance; joints (junctions); insulating concretes; polyurethane resins; precast concrete; residential buildings.

DOI:

Date: 9/1/1979

Abstract:
The use of exterior sprayed-on insulation and portland cement plaster produces an attractive precast wall panel residence which is capable of effi-cient use of solar and thermal energy by storage in the concrete panels until required. The cavelike in-terior environment created by omission of floor insula-tion leads to better control on the use of thermal energy and lower requirements for equipment. Construction and design are described.