Title: Site Precasting

Author(s): Phillip R. Jackson

Publication: Concrete International

Volume: 1

Issue: 4

Appears on pages(s): 18-23

Keywords: beams (supports); columns (supports); concrete panels; economics; lift slab construction; precast concrete.

DOI:

Date: 4/1/1979

Abstract:
The paper presents a nontechnical but nonetheless practical discussion of the use of site precasting as a construction method. It carries the reader through a logical process to analyze the feasibility of site precasting and alert him to what skills he must have or acquire to successfully implement his decision.