Title: Self-Compacting Concrete: Expanding the Possibilities of Concrete Design and Placement

Author(s): Philippe Jost and Michael Campion

Publication: Concrete International

Volume: 22

Issue: 4

Appears on pages(s): 31-34

Keywords: admixtures; self-compacting concrete (SCC); advantages of SCC; production of HPC; high range water reducers; flowability; w/cm; properties of fresh concrete; hardened concrete properties; repair with SCC; economics of repair; new technology; durability

DOI:

Date: 4/1/2000

Abstract:
Self-compacting concrete is a revolutionary technology that dramatically reduces the need for vibration consolidation in the placement of concrete. Faster finishing and more rapid placement is possible. Two case studies are provided to demonstrate the successful use of SCC.