Abstract:
Theoretical papers have immediate practical value if they are studied so as to become a part of one’s working knowied 3e. Such papers seldom give direct answers to speci ic questions, but answers to various questions may emerge from detailed consideration of a specific phenomenon. For example, the vol-ume contraction accompanying hydration, considered along with data on the characteristics and behavior of evaporable water in cement paste, gives useful information pertaining to curing methods and concrete durability.