Erosion of Concrete by Cavitation and Solids in Flowing Water

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Erosion of Concrete by Cavitation and Solids in Flowing Water

Author(s): Walter H. Price

Publication: Journal Proceedings

Volume: 43

Issue: 5

Appears on pages(s): 1009-1024

Keywords: none

DOI: 10.14359/8771

Date: 5/1/1947

Abstract:
High velocity water jet and shot-blast tests which were made to determine the effects of mix propor-tions, curing, absorptive form lining, air entrainment, and surface finish on the erosion resistance of concrete are described. Examples of erosion failures in hydraulic structures by wear and cavitation and methods of repair are included.