Title: Painting Interior Concrete Surfaces : The Experience of One Organization

Author(s): T. H. Chisholm

Publication: Journal Proceedings

Volume: 43

Issue: 4

Appears on pages(s): 913-916

Keywords: none

DOI: 10.14359/8768

Date: 4/1/1947

Abstract:
Twenty-five years’ experience in painting the interior of concrete buildings has demonstrated that if a few simple precautions are taken, it offers no more difficulty than does the painting of wood or other materials. Paper describes the practices of the Hydro-Electric Power Commission of Ontario which have prompted this conclusion.