Effect of Use of Blended Cements and Vinsol Resin-Treated Cements on durability of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Use of Blended Cements and Vinsol Resin-Treated Cements on durability of Concrete

Author(s): W. F. Kellermann

Publication: Journal Proceedings

Volume: 42

Issue: 6

Appears on pages(s): 681-688

Keywords: none

DOI: 10.14359/8736

Date: 6/1/1946

Abstract:
Presents a part of the results obtained from an investigation of the durability of concrete, by the Public Roads Administration using blends of portland cements with natural cements (86 percent and I4 percent by weight, respectively) and Vinsol resin treated cements. Results presented in this contrlbution have a bearing on resistance to freezing and thawing tests, especially because of unusual results of a prolonged interruption of the daily freezing and thawing cycle.