Homogeneity of Air Entraining Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Homogeneity of Air Entraining Concrete

Author(s): Henry L. Kennedy

Publication: Journal Proceedings

Volume: 42

Issue: 6

Appears on pages(s): 641-644

Keywords: none

DOI: 10.14359/8729

Date: 6/1/1946

Abstract:
Reports studies of the homogeneit o f air-entraining concrete by means of testing for resistnance to abrasion. An air-entraining agent was used with no added accelerators, dispersing agents or gas forming materiaIs. Since air entrainment has a tendency to eliminate bleeding of concrete it is only reasonable to believe that such concretes are more homogeneous the top surface (of a slab) would have the same strength and density characteristics as the bottom surface. Plotted data show that there is pro-gressive increase in abrasion loss in specimens as air content increases beyond 6 percent.




  

Edit Module Settings to define Page Content Reviewer