Experiences With Air-Entraining Cement in Central-Mixed Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experiences With Air-Entraining Cement in Central-Mixed Concrete

Author(s): Alexander Foster, Jr.

Publication: Journal Proceedings

Volume: 42

Issue: 6

Appears on pages(s): 625-628

Keywords: none

DOI: 10.14359/8727

Date: 6/1/1946

Abstract:
Reports studies by Warner Co. with central-mixed concrete using air-entraining cement over 2 1/2 -years. Following experimental work, more than 30,000 cu y of air-entrained concrete, chiefly of low-slump, plastic mix were used for pavements and other highway work. Studies included effect of truck-mixer or agitator action, closed drum and open top equipment, on hauls up to 45 min. No significant differences in slump or air entrainment (2 1/2 to 3 percent) were found. The chief problem is in added storage requirements to meet specifications permitting no admixtures and those demanding air entrainment.