Recent Experiences with Air-Entraining Portland Cement Concrete in the Northeastern States

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Recent Experiences with Air-Entraining Portland Cement Concrete in the Northeastern States

Author(s): L. E. Andrews

Publication: Journal Proceedings

Volume: 42

Issue: 6

Appears on pages(s): 621-624

Keywords: none

DOI: 10.14359/8726

Date: 6/1/1946

Abstract:
Describes preliminary studies . and current practice in the northeastern states in the reduction of frost action on concrete paving and other projects (roads, streets, airport pavements and hangars, bridges, and buildings); mix proportioning, methods of determining air content, and field control. Specifications tend to limit air content to 3 to 6 percent rather than fix amount of air-entraining agent used.