Title: Maintenance and Repair of Concrete Bridges on the Oregon Highway System

Author(s): G. S. Paxson

Publication: Journal Proceedings

Volume: 42

Issue: 11

Appears on pages(s): 105-114

Keywords: none

DOI: 10.14359/8705

Date: 11/1/1945

Abstract:
Descripes types of concrete disintegration and methods and materials used in Oregon, for repair and replacement and for protection against further deterioration.