Title: Field Use of Cement Containing Vinsol Resin

Author(s): Charles E. Wuerpel

Publication: Journal Proceedings

Volume: 42

Issue: 9

Appears on pages(s): 49-82

Keywords: none

DOI: 10.14359/8704

Date: 9/1/1945

Abstract:
The results obtained from 22,398 test specimens manufactured in connection with extensive construction, principally during 1941-1944, are presented to-gether with a discussion of the experience with handling concrete containing over 2,000,OOO barrels Vinsol resin cement during this period in I68 structures. Comparisons are drawn between concrete made with plain cement and with cement interground with Vinsol resin as they affect the compressive and flexural strength, the unit weight and the mixing, placing, and finishing operations. See also 40-25, 40-26, 41-5, 42-15, and 42-24 42-38.