Lapped Bar Splices in Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Lapped Bar Splices in Concrete Beams

Author(s): Ralph W. Kluge and Edward C. Tuma

Publication: Journal Proceedings

Volume: 42

Issue: 9

Appears on pages(s): 13-34

Keywords: none

DOI: 10.14359/8702

Date: 9/1/1945

Abstract:
An investigation was conducted to determine the general behavior and strength of lapped bar splices which varied in length and method of splicing. The maximum bond resistance developed in the splice and the slip of bar was determined for two types end sizes of reinforcement. The resulting data clearly Illustrated the manner in which the stress was transferred from one lapped bar to the other and the relative merits of the two types of bars as well as the effectiveness of the two methods of splicing was shown.