Title: Freezing and Thawing Tests of Concrete Made With Different Aggregates

Author(s): Stanton Walker

Publication: Journal Proceedings

Volume: 40

Issue:

Appears on pages(s): 573-580

Keywords:

DOI: 10.14359/8672

Date: 6/1/1944

Abstract:
Summarizes information on freezing and thawing tests of concrete made with different coarse aggregates and describes a durability factor which may be calculated as a function of the cycles of freezing and thawing and their effect on the modulus of elasticity of the concrete as measured dynamically.