Title: Navy Installations of Protective Linings for Concrete Tanks Containing Liquid Fuels

Author(s): Morris A, Spamer

Publication: Journal Proceedings

Volume: 40

Issue:

Appears on pages(s): 417-428

Keywords:

DOI: 10.14359/8666

Date: 4/1/1944

Abstract:
Reviews the experiences of the Bureau of Yards and Docks in the application of about 2 1/2 million sq ft of protective linings for concrete tanks to contain diesel oil and aviation gasoline. As other literature on this subject deals almost entirely with research work, this paper reports field experience with a summary of results to date in this comparatively new field particularly as the linin by the Navy is the only one of considera b le magnitude that has presently been completed.