High Pressure Steam Curing

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: High Pressure Steam Curing

Author(s): ACI Committee 716

Publication: Journal Proceedings

Volume: 40

Issue:

Appears on pages(s): 409-416

Keywords:

DOI: 10.14359/8665

Date: 4/1/1944

Abstract:
The committee defines high-pressure steam curing in terms of performance in reduced shrinkage of concrete products; arrives at I I conclusions as to the characteristics of concrete products cured by high-pressure steam and appends a considerable list of references as background for the report.