Alkali Etching Tests on Concrete Aggregates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Alkali Etching Tests on Concrete Aggregates

Author(s): Willard H. Parsons and Herbert Insley

Publication: Journal Proceedings

Volume: 40

Issue:

Appears on pages(s): 229-244

Keywords:

DOI: 10.14359/8658

Date: 1/1/1944

Abstract:
A test for determining the reactivity of an aggre- gate with high-alkali cements is described, which consists of microscopic examination of polished sur- faces of rocks and minerals after etching in various alkaline hydroxide and sulfate solutions. Pure opal, opaline chert and opaline limestone are readily etched, while volcanic glass, certain feldspars, chal- cedony, calcite, and dolomite are slightly etched under some of these test conditions. Photomicrographs of etched rocks and minerals are included.