Title: Proposed Recommended Practice For the Design of Concrete Mixes

Author(s): ACI Committee 613

Publication: Journal Proceedings

Volume: 40

Issue:

Appears on pages(s): 93-116

Keywords:

DOI: 10.14359/8651

Date: 11/1/1943

Abstract:
The nature of the report is implicit in the title. With three amendments and some editorial revision (see Apr. 1944 ACI Journal News Letter p. 3) the report was approved for adoption as an ACI Stand- ard and ratified by letter ballot July 28, 1944,