Long Span Concrete Roof Construction
Author(s):
C. H. Mayer
Publication:
Journal Proceedings
Volume:
39
Issue:
Appears on pages(s):
389-396
Keywords:
DOI:
10.14359/8634
Date:
4/1/1943
Abstract:
Shows the reinforced concrete roof design used by the author during the last 25 years for economy and speed. It is of special interest in its minimum use of critical materials in these times. The notable fea- ture of the design is a simple Howe truss whose top chord members support a continuous light and ventilation. monitor for