The Effect of Change in Moisture-Content on the Crepe of Concrete Under a Sustained Load

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Effect of Change in Moisture-Content on the Crepe of Concrete Under a Sustained Load

Author(s): Gerald Pickett

Publication: Journal Proceedings

Volume: 38

Issue:

Appears on pages(s): 333-356

Keywords:

DOI: 10.14359/8607

Date: 2/1/1942

Abstract:
The amount and rate of plastic flow in concrete under load has been found to depend on the rate of drying. This paper shows by mathematical analysis that this is a natural consequence of nonuniform shrinkage and a nonlinear stress-creep relationship. It further shows that shrinkage cannot account for additional creep unless inelastic strain not proportional to stress is produced. signed to test the Results from experiments decrete are reported. applicability of the theory to con-Presidents