The Effect of Belt Transportation on Concrete Transportation on Concrete Aggregate Grading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Effect of Belt Transportation on Concrete Transportation on Concrete Aggregate Grading

Author(s): Gordon L. Williams

Publication: Journal Proceedings

Volume: 38

Issue:

Appears on pages(s): 329-332

Keywords:

DOI: 10.14359/8606

Date: 2/1/1942

Abstract:
Steps in the solution of the problem presented by breakage of graded concrete aggregate through 26 flights of a 91/2-mile belt conveyor which took aggregate from the gravel plant at Redding, Calif., to the mixing plant for Shasta Dam.