Title: Saving Steel In Reinforced Concrete Design

Author(s): R. L. Bertin

Publication: Journal Proceedings

Volume: 38

Issue:

Appears on pages(s): 281-288

Keywords:

DOI: 10.14359/8602

Date: 1/1/1942

Abstract:
Proposes the prompt modification of the Institute’s Building Regulations for Reinforced Concrete (ACI 318-41) in furtherance and support of a proposed National Emergency Code for the conservation of steel and other strategic materials, chiefly for defense construction where time is urgent and steel short; that working stresses be liberalized, live loads reduced, plain concrete encouraged and the most modern methods of design applied.