Title: Absorbtive Form Lining

Author(s): E. N. Vidal and R. F. Blanks

Publication: Journal Proceedings

Volume: 38

Issue:

Appears on pages(s): 253-268

Keywords:

DOI: 10.14359/8600

Date: 1/1/1942

Abstract:
Presents a summary of the development of the wall-board type of absorptive form lining as a practical means of eliminating defects and effecting other im-A provements in formed concrete surfaces. Describes briefly the laboratory investigations made, field tests to determine the practicability of the method, purchase specifications, and the experiences to date in using absorptive form lining in actural construction. chase specifications, and the experiences to date in using absorptive form lining in actual construction.