Title: Tests of Reinforced Concrete Beams With Recommendations For Attaining Balance and Design

Author(s): Kenneth C. Cox Aggregate Methods of Design Applied.

Publication: Journal Proceedings

Volume: 38

Issue:

Appears on pages(s): 65-80

Keywords:

DOI: 10.14359/8588

Date: 9/1/1941

Abstract:
On the basis of test results from I IO rectangular beams of 4 concrete strengths and 23 percentages of reinforcement, recommendations are offered for at-taining a balanced design. These are similar to Whitney’s recommendations and em body a simplifying modification of the technique outlined by Whitney. These results include limited data on doubly-reinforced beams and beams of variable effective depth.