The Design and Control of Paving Concrete in Iowa

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Design and Control of Paving Concrete in Iowa

Author(s): Bert Myers

Publication: Journal Proceedings

Volume: 37

Issue:

Appears on pages(s): 577-588

Keywords: none

DOI: 10.14359/8572

Date: 4/1/1941

Abstract:
Reports Iowa Highway Commission practices over 20 years, in the design and control of paving concrete: ( I ) The design of proportions to make the most eco- nomical use of the aggregates available, particularly mixtures containing a high ratio of mortar to coarse aggregate, (2) the introduction of the practice of weighing aggregates for paving concrete, (3) improve- ments in methods for the control of thickness of pave- ment slab, (4) design of equipment for accurate con- trol of measurement of mixing water, (5) detailed methods for control of proportions.