Columns With High Yield Point Reinforcement Designed Under the A. C. I. Code

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Columns With High Yield Point Reinforcement Designed Under the A. C. I. Code

Author(s): Thor Germundsson

Publication: Journal Proceedings

Volume: 37

Issue:

Appears on pages(s): 569-576

Keywords: none

DOI: 10.14359/8571

Date: 4/1/1941

Abstract:
The customary type of reinforced concrete column is not too satisfactory for large loads. An improvement is proposed by means of which columns may be made smaller and more economical. At the same time, their size may be kept the same throughout a tall building, 20 in. being considered the optimum size for all col- umns carrying up to l,OOO,OOO lb. This results in stand- ardization of design, detailing and erection of floor construction on various levels. To accomplish that it is proposed to use eight bars in each column, the maximum size of bars being 2 in. round and their yield point stress 75,000 psi.