Concrete Control On The Pennsylvania Turnpikel

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Control On The Pennsylvania Turnpikel

Author(s): I. L. Tyler

Publication: Journal Proceedings

Volume: 37

Issue:

Appears on pages(s): 361-376

Keywords: none

DOI: 10.14359/8558

Date: 2/1/1941

Abstract:
Deals with problems encountered in controlling quality of paving concrete on a large project, the Pennsylvania Turnpike, constructed in record time. Procedures adopted for maintaining such control are briefly discussed. Suggesting that uncontrolled mixing water has been the important factor in most of the recorded failures of concrete structures, the paper directs particular attention to the phase of construc- tion having to do with its control. Data are presented which indicate that the actual amount of mixing water in concrete may be considerably greater than is gen- erally supposed. Effects of type of concrete placing equipment on quality of concrete and some effects of construction practices and procedures are considered. Suggestions are offered which may be of value in preparing paving specifications.