Correlation Between Rapid Immersion And Standard Four Cycle Per Day Freezing And Thawing Tests

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Correlation Between Rapid Immersion And Standard Four Cycle Per Day Freezing And Thawing Tests

Author(s): E. R. Dawley

Publication: Journal Proceedings

Volume: 37

Issue:

Appears on pages(s): 157-160

Keywords: none

DOI: 10.14359/8549

Date: 11/1/1940

Abstract:
Progress report of an investigation attempting to shorten the time required to measure resistance of rock to freezing and thawing. The rapid method consists of a direct immersion of the specimen in freezinq solutions for IO min. then thawina. in running water for 5 min, wiping, and returning to the freezing solution. Two solutions, Skellvsolve F and mercury, were used. Tests of three kinds of rock by the standard method and the rapid method are described. Disintegration of the specimens was slightly more rapid using the rapid method. The standard method caused more damage by splitting.