Comparison Of The Physical And Mechanical Properties Of Hand Rodded And Vibrated Concrete Made With Different Cements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Comparison Of The Physical And Mechanical Properties Of Hand Rodded And Vibrated Concrete Made With Different Cements

Author(s): George W. Washa

Publication: Journal Proceedings

Volume: 36

Issue: 6

Appears on pages(s): 617-646

Keywords: none

DOI: 10.14359/8541

Date: 6/1/1940

Abstract:
Presents results of a comprehensive series of tests on vibrated and hand-rodded *concrete. The variables for each method of placement are five different mixes and five different cements. Particular attention has been paid to the lean mixes, the leanest vibrated mix being I :6:12 by weight, wrth only 2.2 sacks of ce- ment per cu d of concrete. The results obtained indi- cate the e ects of the variables on compressive ff strength, permeability, specific weight, absorption, linear changes due to alternate heating and water soaking, modulus of elasticity, Poisson’s ratio, shrink- age, and plastic flow.