The Properties Of Concrete Mixes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Properties Of Concrete Mixes

Author(s): R. F. Blanks, E. N. Vidal, W. H. Price, And F. M. Russell

Publication: Journal Proceedings

Volume: 36

Issue: 4

Appears on pages(s): 433-476

Keywords: none

DOI: 10.14359/8531

Date: 4/1/1940

Abstract:
An attempt to assemble in exemplified form the known properties, factors, and relationships pertaining to concrete In the plastic state. Details of con- crete proportioning procedure are not included, and reference is made to the properties of hardened concrete only when its requirements directly affect or predetermine certain properties of the fresh concrete. The introduction includes a brief discussion of the concrete proportioning problem and a highly con- densed account of the more important historical de- velopments. The second section discusses the known properties of concrete mixes and related facts, and presents supporting data and information from the literature and from unpublished records.