Tests On Concrete Maonry Units Using Tamping And Vibration Molding Methods

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tests On Concrete Maonry Units Using Tamping And Vibration Molding Methods

Author(s): Kurt F. Wendt and Paul M. Woodworth

Publication: Journal Proceedings

Volume: 36

Issue: 11

Appears on pages(s): 121-164

Keywords: none

DOI: 10.14359/8517

Date: 11/1/1939

Abstract:
Results of a comprehensive,. correlated series of tests on concrete masonry units made with seven different aggregates, cinders, Haydite, limestone, Pott- sco, sand and gravel, Superock, and Waylite. Comparative data show the effect of two different types of molding, vibration, and tamping on compressive strength, absorption, capillarity, specific weight, durability, volume change, and thermal expansion coef-ficient for each aggregate. Similar comparative data are presented for variations in cement content for each aggregate.