Title: Design Coefficients For Building Frames

Author(s): A. J. Boase and J. T. Howell

Publication: Journal Proceedings

Volume: 36

Issue: 9

Appears on pages(s): 21-36

Keywords: none

DOI: 10.14359/8512

Date: 9/1/1939

Abstract:
Presents a short, easily applied, readily understood method for analysis of buildinq frames by principles of continuity to conform to modern code demands giv-ing all accuracy necessary for commercial and practical requirements. Moment coefficient tables iving maximum and minimum moment coefficients for build-ing frames of variable spans are given, with examples of their use.