Factors Affecting The Resistance To Freezing And Thawing Of Vibrated Concrete Made Of Crushed Dolomite

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Factors Affecting The Resistance To Freezing And Thawing Of Vibrated Concrete Made Of Crushed Dolomite

Author(s): M. O. Withey

Publication: Journal Proceedings

Volume: 35

Issue: 6

Appears on pages(s): 553-560

Keywords: none

DOI: 10.14359/8509

Date: 6/1/1939

Abstract:
Reports effect of 150 cycles of freezing and thawing on the flexural and compressive strength of 100 concrete prisms. Little or no damage was suffered byconcrete with 0.54 water-cement ratio, by weight, containing 43/4 sacks of cement per cu yd. The flexure test was a far more sensitive measure of resistance to freezing and thawing than the compression test.