Corner Effects In Rigid Frames

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Corner Effects In Rigid Frames

Author(s): Joseph A. Wise

Publication: Journal Proceedings

Volume: 35

Issue: 1

Appears on pages(s): 189-192

Keywords: none

DOI: 10.14359/8485

Date: 1/1/1939

Abstract:
The moments in beams at the face of columns in rigid frames is less than the moment at the intersection of the center lines of the members. Also, the zone of intersection of the members, tends to cause an increase in stiffness at the ends. The problem is discussed and tentative method of obtaining the moment at face of column is proposed.