Overvibration And Revibration Of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Overvibration And Revibration Of Concrete

Author(s): Lewis H. Tuthill and harmer E. Davis

Publication: Journal Proceedings

Volume: 35

Issue: 9

Appears on pages(s): 41-48

Keywords: none

DOI: 10.14359/8477

Date: 9/1/1938

Abstract:
Effects of overvibration are rarely encountered in concrete of medium and the drier consistencies, in the wetter consistencies horizontal stratification may result with detriment to durability. Tests show that aslong as the concrete has not become so stiff that re-vibration will not restore plasticity, revibration bene-fits, does not harm concrete.