Title: Concrete Wearing Surfaces For Floors

Author(s): ACI Committee 804

Publication: Journal Proceedings

Volume: 35

Issue: 9

Appears on pages(s): 21-32

Keywords: none

DOI: 10.14359/8475

Date: 9/1/1938

Abstract:
Data and faces for ha recommendations on concrete floor surrd wear. with record of new accelerated tests; suggests a specification outline for materials and workmanship both held within narrow limits. A departure from usual practice is presented for criticism.