Title: Field Survey Of Mass Concrete

Author(s): F. R. McMillan

Publication: Journal Proceedings

Volume: 34

Issue: 5

Appears on pages(s): 561-572

Keywords: none

DOI: 10.14359/8468

Date: 5/1/1938

Abstract:
In this survey, Committee 108 attempts to determine to what extent the properties peculiar to mass concrete. are responsible for conditions observed massive structures. Effect of improved workmanship and changes in materials on properties of concrete are noted. These effects are demonstrated by descriptions of Crystal Springs, Elephant Butte, Arrow-rock, Morris, and Boulder dams, and others unidentified.