Cracking In Mass Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cracking In Mass Concrete

Author(s): R. F. Blanks, H. S. Meissner, and C. Rawhouser

Publication: Journal Proceedings

Volume: 34

Issue: 3

Appears on pages(s): 477-496

Keywords: none

DOI: 10.14359/8463

Date: 3/1/1938

Abstract:
Includes descriptive matter and tests on. the cause and control of cracking, temperature variation and thermal stress and volume change, based on des ign and research work of the Bureau of Reclamation. Structures studied include Owyhee, Boulder, Grand Coulee, Norris, Bartlett, and Morris dams and other smaller dams. Shrin kaqe studies of test bars and cylinders are described and results indicated. The most effective single method for improving crack- ing conditions is the use of low-heat or portland- pozzolan cement.