Classification Of Admixtures As To Pozzolanic Effect By Means Of Compressive Strength Of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Classification Of Admixtures As To Pozzolanic Effect By Means Of Compressive Strength Of Concrete

Author(s): F. R. Mc Millan And T. C. Powers

Publication: Journal Proceedings

Volume: 34

Issue: 11

Appears on pages(s): 129-144

Keywords: none

DOI: 10.14359/8445

Date: 11/1/1937

Abstract:
Strength test data are used to indicate the effect of the following admixtures: bentonite, Tripoli silica, California oumicite. diatomaceous earth. crvstalline talc, hydrated lime: Kansas pumicite, Magnolia cei merit, blast furnace slag, and hydraulic lime. Strenath is considered as an index sample analysis of data is to pozzolanic action, and given in an appendix.