Calculation Of Temperature Distribution In a Succession Of Lifts Due To Release Of chemical Heat

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Calculation Of Temperature Distribution In a Succession Of Lifts Due To Release Of chemical Heat

Author(s): Robert E. Glover

Publication: Journal Proceedings

Volume: 34

Issue: 11

Appears on pages(s): 105-116

Keywords: none

DOI: 10.14359/8443

Date: 11/1/1937

Abstract:
Exact and rapid calculations of temperature distribution in successive lifts are obtained by synthesis from Kelvin’s instantaneous surface source. Integrals are arranged for graphical evaluation with the aid of a planimeter. A mathematical device is introduced to simplify and expedite the graphical work. The first part of the paper deals with diffusion of the heat previously generated, the second accounts for heat released by chemical action, and a third part deals with the effect of external temperature changes.