Design Of Reinforced Concrete Members Under Flexure Or Combined Flexure And Direct Compression

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design Of Reinforced Concrete Members Under Flexure Or Combined Flexure And Direct Compression

Author(s): Charles S. Whitney

Publication: Journal Proceedings

Volume: 33

Issue: 3

Appears on pages(s): 483-498

Keywords: none

DOI: 10.14359/8429

Date: 3/1/1937

Abstract:
Presents a rational method for the proportioning of arch ribs, rectangular columns under eccentric load, and beams which recognizes the plasticity of the concrete and its effect on the stress-strain relationship. Formulas are given which predict the ultimate strength of members based on the cylinder strength of the concrete and yield strength of the steel independent of the ratio of their moduli of elasticity.