The New Federal Specifications For Portland Cements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The New Federal Specifications For Portland Cements

Author(s): Ben Moreell

Publication: Journal Proceedings

Volume: 33

Issue: 3

Appears on pages(s): 435-455

Keywords: none

DOI: 10.14359/8427

Date: 3/1/1937

Abstract:
Gives the history of development of American portland cement specifications and reasons for de-velopment of the new Federal Specifications for nonstandard portland cements. He describes the principal features of the four new specifications for normal portland cement, high-early-strength cement, moderate heat of hardening cement, and sulfate-resisting cement and discusses practical features of manufacture and use of the new cements.