A Study Of Sub-Aqueous Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Study Of Sub-Aqueous Concrete

Author(s): Arthur R. Anderson

Publication: Journal Proceedings

Volume: 33

Issue: 1

Appears on pages(s): 339-346

Keywords: none

DOI: 10.14359/8422

Date: 1/1/1937

Abstract:
A comparison of two methods of placing water concrete, the tremie method and 8 under- rop-bot-tom bucket method. The strengths of the tremie concrete are compared with similar concrete deposited in air under standard control conditions. The effect of qradinq of aggregates, quality of cement and workability on subaqueous concrete was also studied. The strengths obtained from sub-aqueous concrete were lower than the strengths obtained from the same concrete not deposited under water. On an average, tremie concrete was I7 percent stronger than concrete placed with a drop-bottom bucket.