Title: Earthquakes And Reinforced -Concrete

Author(s): Jacob J. Creskoff

Publication: Journal Proceedings

Volume: 33

Issue: 1

Appears on pages(s): 223-249

Keywords: none

DOI: 10.14359/8415

Date: 1/1/1937

Abstract:
Investigates the distribution and frequency of earthquakes in the United States, theory of earthquake causation, nature and effect of earthquake vibrations on structures, statical and dynamical design of earthquake-resistant structures, and the characteristics of reinforced concrete which make it par-ticularly suitable for use in earthquake-resistant construction