Portland -Puzzolan Cement As Used In The Bonneville Spillway Dam

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Portland -Puzzolan Cement As Used In The Bonneville Spillway Dam

Author(s): R. R. Clark and H. E. Brown

Publication: Journal Proceedings

Volume: 33

Issue: 1

Appears on pages(s): 183-221

Keywords: none

DOI: 10.14359/8414

Date: 1/1/1937

Abstract:
A description of concrete studies and construction of the Bonneville Dam. The method of construction consists of two principal steps in which one half is built in one working season between summer floods. There are about 500,000 cu yd of mass concrete and another 100,000 cu yd of reinforced concrete. Topics covered include cement investigation and selection, special cement specifications, concrete studies, stress analysis, and construction. The Investigation and use of Portland-pozzolan cement for the dam is described in detail. Emphasizes the control of mass concrete from the design standpoint.